E42-287 · Stress Concentration · Load-Carrying Weld · ★★
Load-carrying weld toe un-ground becomes fatigue initiation; crack 25mm; 3 cracks per month
[Sharp Toe] Sharp weld-toe angle; un-ground; stress concentration Kt=2.0.
[Fatigue] Alternating σ=200MPa; life 60k cycles (design 150k); initiates at toe.
[Design Omission] Toe not ground; not blended; safety factor 1.3 (should be ≥1.8).
1) Grind weld toe smooth R3;
2) Peen toe to relieve stress;
3) Control reinforcement ≤1mm;
4) Change fillet joint to butt to lower stress;
5) MPI each location;
6) Optimize loading to avoid stress peak;
7) Shot peen;
8) Periodic NDE.
GB/T 50661-2011