E42-290 · Stress Concentration · Welded Perforated Plate · ★★
Welded perforated plate (δ=20); hole edge unstrengthened tensile crack 40mm; 2 cracks per month
[Hole Edge] Hole edge unstrengthened; stress concentration Kt=2.4.
[Fatigue] Tensile σ=220MPa; life 80k cycles (design 200k); initiates at hole edge.
[Design Omission] Hole not reamed; not chamfered; safety factor 1.3 (should be ≥1.8).
1) Ream hole edge and chamfer C1;
2) Roll-strengthen hole mouth;
3) Add reinforcing pad (width 3d);
4) MPI each location;
5) Limit load to 90% rated;
6) Material re-test;
7) Shot peen;
8) Periodic NDE.
GB/T 150.3-2011