Knowledge Base › Structural Design Error Case Study › Hydraulic Cylinder Piston-Rod Runout Groove Sharp Corner Fracture

Hydraulic Cylinder Piston-Rod Runout Groove Sharp Corner Fracture

E42-411 · Stress Concentration · HSG-80 Hydraulic Cylinder Piston Rod · ★★★

Problem Description

HSG-80 cylinder piston rod (Φ80) fractures at runout groove r=0.3mm; cylinder loses pressure; 3 replaced per month

Root Cause

[Sharp Corner] Runout groove r=0.3mm (should be ≥1.5mm); stress concentration Kt=3.2. [Fracture] Alternating tension-compression σ=320MPa exceeds fatigue; breaks at groove bottom. [Design Omission] Not roll-strengthened; fillet uncontrolled; safety factor 1.1 (should be ≥2.0).

Corrective Solution

1) Increase runout groove r to ≥1.5mm;
2) Roll-strengthen groove bottom;
3) Quench-and-temper piston rod HB280;
4) Magnetic-particle inspect each shaft;
5) Limit load to 90% rated;
6) Add cushion stroke;
7) Dynamic balance;
8) Replace at end of life.

Checklist

Reference

GB/T 13342-2007

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL