E42-127 · Thermal Distortion & Thermal Stress · Bed Casting with Steel-Inlaid Guide Rail · ★★
After warm-up the differential expansion of the steel-inlaid guide and the cast iron base skews the straightness by 0.03mm
[Expansion Difference] Steel has a linear expansion coefficient of 12e-6 against 10e-6 for cast iron, and at ΔT=15℃ the length difference bends the guide.
[Skew] The constraint at the bonding interface makes the guide crown by 0.03mm.
[Design Omission] No expansion compensation was provided and materials of similar expansion were not selected.
1) Select steel and base materials with similar expansion coefficients;
2) Leave a temperature expansion gap at the bonding interface;
3) Carry out a coupled thermal-structural finite element analysis;
4) Re-measure the straightness by laser after warm-up;
5) Add temperature compensation corrections;
6) Control the temperature rise ΔT≤10℃;
7) Arrange the datum surfaces symmetrically;
8) Include thermal skew in the accuracy acceptance.
JB/T 2256 Jig Boring Machines — Inspection of Accuracy