Knowledge Base › Structural Design Error Case Study › Hammer Crusher Hammer Head Broken Shank Fly-Out

Hammer Crusher Hammer Head Broken Shank Fly-Out

E42-305 · Impact and Overload Fracture · PCK1010 Hammer Crusher Hammer Head · ★★★

Problem Description

PCK1010 hammer crusher hammer head (50kg) broke shank and flew out at high speed; 3 shutdowns per month

Root Cause

[Centrifugal Overload] Linear speed v=45m/s; centrifugal force F=3200N makes shank stress σ=520MPa exceed strength.
[Fatigue] Alternating bending superimposed; short life.
[Design Omission] No dynamic balance verification, shank section too small; safety factor only 1.1 (should be ≥2.0).

Corrective Solution

1) Dynamically balance the hammer rotor to G6.3;
2) Enlarge the shank section to 1.5x original;
3) Change material to high-manganese steel ZGMn13;
4) Weigh and match sets before installation, difference ≤50g;
5) Crack check each shift;
6) Limit overspeed to 10%;
7) Reinforce the guard;
8) Mandatory replacement at end of life.

Checklist

Reference

GB/T 5680-2010