Insufficient Wall Thickness of a Magnesium Alloy Housing Causes Crushing Under Pressure

E42-094 · Insufficient Strength in Lightweight Design · Magnesium Alloy Housing AZ91D · ★★

Problem Symptom

The part crushed under load

Root Cause

[Wall Thickness] A 3mm magnesium alloy wall has insufficient compressive capacity.
[Crushing] The part yielded and crushed.
[Design Omission] Compressive capacity was not checked and the wall was too thin, so the part crushed.

Correct Solution

1) Increase the wall thickness to 5mm;
2) Check the compressive stability;
3) Add ribs for reinforcement;
4) Upgrade the material;
5) Distribute the load;
6) Optimise the mould flow;
7) Carry out a proof pressure test;
8) Make compressive capacity a mandatory calculation.

Checklist

References

GB/T 5153-2016 Wrought Magnesium and Magnesium Alloys

Related 3D models: Ready to build it? Download free 3D models & CAD drawings at MOULDL »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL