Knowledge Base › Structural Design Error Case Study › Magnesium Housing Cracking

Magnesium Housing Cracking

E42-544 · Insufficient Lightweight Strength · Magnesium alloy housing (AZ91) · ★★

Problem Description

Housing wall 1.5, vibration σ=140 exceeding allowable 120, cracked and leaked; 2 pieces scrapped monthly

Root Cause

[Low strength] t=1.5 thin, σ=140>allowable 120, cracked.
[Lightweight] Over-reduced.
[Design Omission] No vibration-strength check, thin wall; safety factor 1.1 (should be ≥1.5).

Corrective Solution

1) Raise wall thickness to 2.5;
2)Ribbing;
3) Vibration-damping design;
4) Crack check each shift;
5) Limit vibration;
6) Upgrade material;
7)NDE;
8) Periodic re-measurement.

Checklist

Reference

GB/T 5153-2016