Welding Residual Stress Causes Warping After Machining

E42-047 · Residual Stress Distortion · Welded Frame · ★★★

Problem Symptom

0.06mm of warping after welding and machining

Root Cause

[Welding Residual Stress] The weld residual stress is σ_r=350MPa.
[Release] Machining away the restraint releases 0.06mm of bending.
[Design Omission] No ageing was applied after welding before finish machining, so the part warped.

Correct Solution

1) Apply ageing after welding;
2) Leave 0.5mm of secondary allowance;
3) Separate the operations to release stress progressively;
4) Apply artificial ageing;
5) Measure the stress;
6) Inspect the distortion;
7) Optimise the process;
8) Write post-weld ageing into the process specification as a mandatory node.

Checklist

References

GB/T 37400 Welded Parts

Related 3D models: Ready to build it? Download free 3D models & CAD drawings at MOULDL »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL