Knowledge Base › Tolerance and Fit Error Case › Process Datum-Transfer Accumulation

Process Datum-Transfer Accumulation

E43-503 · Datum Non-Coincidence · A shaft rough-turned on center holes and finish-turned on the OD, radial run-out 0.08 · ★★★

Problem Description

Rough- and finish-turning datum transfer did not coincide, giving outer-diameter run-out 0.08mm out of tolerance.

Root Cause

[Mechanism] Rough center-hole and finish OD datums do not coincide, so center-hole-to-OD coaxiality error feeds in.
[Calculation] Datum non-coincidence error = center-hole-to-OD coaxiality 0.08, 4× the tolerance of 0.02.
[Design Omission] One datum was not carried through the processes; design defect → radial out of tolerance.

Corrective Solution

1) Finish-turn still on the center holes;
2) Grind center holes to hold coaxiality;
3) Unify the process datum;
4) Tolerance-allocate by datum offset;
5) First-article run-out measurement;
6) Note the datum chain in the process sheet;
7) Reduce datum transfers;
8) First-article run-out measured ≤0.02.

Checklist

Reference

GB/T 1182-2018 GPS — Geometrical tolerancing (form, orientation, location and run-out)