E43-577 · Tolerance Specification and Grade Error · A shoulder transition R marked R2 without tolerance, so the actual R runs 0.5 and stress concentration causes fatigue cracking · ★★★
The shoulder fillet R carries no tolerance; the actual R comes out small at 0.5, raising the stress concentration factor and causing fatigue cracking.
[Mechanism] The shoulder transition fillet radius governs stress concentration; omitting a tolerance lets it run small, sharply raising the stress concentration factor and initiating fatigue cracks.
[Calculation] At R2, Kt ≈ 1.6; at R0.5, Kt ≈ 2.5. The alternating stress amplifies by 56% and the fatigue life drops to one quarter.
[Design Omission] The transition fillet lacks a tolerance and has no lower limit; design defect → stress-concentration cracking.
1) Dimension the transition fillet as R2−0/+0.5 to guarantee at least R2;
2) Control Kt ≤ 1.6 per fatigue requirements;
3) Follow the fillet rules of GB/T 6403.4;
4) On the first article, measure the fillet with an R gauge;
5) Put a lower-limit tolerance on the fillet in the drawing;
6) Use a form tool in machining to hold the R;
7) Polish the fillet to reduce stress;
8) Verify life by fatigue testing.
GB/T 6403.4-2008 Rounding and chamfering of parts