E43-580 · Tolerance Specification and Grade Error · A cast-iron base wrongly specified CT6 instead of CT10, exceeding foundry capability and causing blanks to run out widely · ★★
The casting general tolerance is wrongly set to the tight grade CT6, which sand casting cannot achieve; blanks run out widely and require rework.
[Mechanism] Casting general tolerances are graded CT per GB/T 6414; sand casting capability is about CT10–12, so a CT6 call far exceeds the process capability.
[Calculation] For 100 mm, CT6 is ±0.4, while actual sand-casting capability is ±1.4 (CT11), a 3.5-fold overshoot.
[Design Omission] The casting is given too high a CT grade; design defect → blanks run out widely.
1) Set sand-cast blanks to general tolerance CT11–12;
2) Leave machining allowance (RMA) on machined surfaces;
3) Follow the casting dimensional tolerances of GB/T 6414;
4) Call out a finer grade on critical surfaces after machining;
5) On the first article, measure the blank dimensional distribution;
6) Mark the CT grade and RMA on the drawing;
7) The CT grade may be raised if molding accuracy is improved;
8) Sample-inspect blanks in batches.
GB/T 6414-2017 Castings — Dimensional tolerances, geometrical tolerances and machining allowances