E43-605 · Surface Roughness Mismatched with Fit · A gear ring interference bore ∅120 where the design specified Ra 0.8 but actual was Ra 3.2, flattening peaks after pressing and defeating the interference · ★★★
The interference-fit face was too rough (Ra 3.2); asperities were flattened after pressing, so effective interference was lost and the gear ring loosened and slipped.
[Mechanism] During press-fitting, microscopic surface peaks are flattened; the rougher the surface, the more effective interference is lost, until residual interference cannot transmit torque.
[Calculation] Rz ≈ 5 Ra = 16 μm; effective interference loss ≈ 1.2 (Rz_hole + Rz_shaft) = 1.2 × 32 = 38 μm; with nominal interference 50 μm, only 12 μm remains and the joint loosens.
[Design Omission] The interference-face roughness was left uncontrolled; this design defect leads to insufficient effective interference and loosening.
1) Finish-grind the interference face to Ra 0.8 to reduce peak height;
2) Per GB/T 131, set Ra ≤ 0.8 for interference fits;
3) Compensate nominal interference for the 1.2 (Rz1 + Rz2) loss;
4) On the first article, measure Ra and the press-fit force curve;
5) Annotate Ra 0.8 on the mating face on the drawing;
6) Do not rough-turn after grinding;
7) Monitor retention force during pressing;
8) Verify by torque transmission testing.
GB/T 131-2006 Geometrical product specifications — Surface texture designation