Knowledge Base › Tolerance and Fit Error Case › Too-Smooth Substrate Before Coating Causing Poor Paint Adhesion

Too-Smooth Substrate Before Coating Causing Poor Paint Adhesion

E43-653 · Surface Roughness Mismatch with Fit · A structural coating surface designed for blasted Ra12.5 but actually Ra1.6, too smooth for paint anchoring, causing blistering and peeling · ★

Problem Description

The substrate was left too smooth at Ra1.6 before coating; mechanical anchoring of the paint film was insufficient, and it blistered and peeled in humid conditions.

Root Cause

[Mechanism] Paint adhesion relies on mechanical anchoring into the substrate; an over-smooth surface anchors poorly, and moisture penetrates the interface in humid service, causing blistering and peeling.
[Calculation] At Ra1.6 the adhesion is about 40% lower than at blasted Ra12.5, and blistering appears early in salt-spray/humidity testing.
[Design Omission] The surface was left too smooth without blasting before coating; design defect → paint peeling.

Corrective Solution

1) Blast to Sa2.5 and Ra12.5 before coating;
2) Set the substrate roughness per the coating process;
3) Degrease and derust before coating;
4) Inspect the first article for Ra and adhesion;
5) Mark the blast grade on the drawing;
6) Match the primer;
7) Do a cross-cut adhesion test;
8) Verify by salt-spray testing.

Checklist

Reference

GB/T 131-2006 Geometrical product specifications — Surface texture designation

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »