E43-656 · Surface Roughness Mismatch with Fit · A piston ring OD designed for Ra0.4 but actually Ra1.6, giving poor sealing against the cylinder wall, high blow-by and oil consumption · ★★
The piston ring OD was left at Ra1.6, so its sealing contact with the cylinder wall was poor; blow-by increased and oil consumption ran high.
[Mechanism] The piston ring OD seals against the cylinder wall; a too-rough face makes the sealing line discontinuous, allowing gas blow-by and leaving oil not fully wiped, which raises oil consumption.
[Calculation] The discontinuous sealing line at Ra1.6 increases blow-by and leaves oil un-wiped; oil consumption is about 20% higher than at Ra0.4.
[Design Omission] The piston ring OD was left too rough; design defect → blow-by and oil consumption.
1) Grind the piston ring OD to Ra0.2~0.4;
2) Chrome-plate or nitride the ring face for wear resistance;
3) Set ring Ra per sealing requirements;
4) Inspect the first article for Ra and blow-by rate;
5) Mark the ring OD Ra on the drawing;
6) Lap and run in the ring against the bore;
7) Match ring tension;
8) Measure blow-by and oil consumption on the test rig.
GB/T 131-2006 Geometrical product specifications — Surface texture designation