E43-710 · Taper and angle fit error · A thin-walled taper sleeve pressed at 1.5× the design force, going out-of-round after pressing with roundness growing from 0.005 to 0.02mm · ★★★
The press-fit force on a thin-walled taper sleeve was 1.5× the design value; the thin wall saw excessive radial force from the taper, the sleeve went out-of-round after pressing, roundness grew from 0.005mm to 0.02mm, and fit accuracy was lost.
[Mechanism] Press-fitting a thin-walled part on an interference taper generates large radial force; when the press force is excessive, the elastic deformation exceeds the elastic limit, leaving residual out-of-round after unloading.
[Calculation] A 1.5× press force pushes the thin wall past its elastic limit, leaving 0.015mm residual out-of-round, which exceeds the 0.005mm roundness requirement.
[Design Omission] The thin-walled taper sleeve had too much interference or too high a press force; this design defect → leads to out-of-round after pressing.
1) Recompute the interference and press force based on the thin-wall stiffness;
2) Reduce the interference, or switch to hot assembly to cut the radial force;
3) On the first article, measure roundness after pressing;
4) Add a support ring to reduce thin-wall deformation;
5) Monitor the press force;
6) Taper contact rate ≥80%;
7) State the interference and process on the drawing;
8) Recheck roundness.
GB/T 1800.1-2020 Geometrical product specifications (GPS) - Limits and fits