E43-762 · Thread Tolerance and Fit Error · Long-term fretting on vibrating equipment wears the flanks, loosens the pitch-diameter fit, and keeps decaying preload so frequent retightening is needed · ★★★
Threaded joints on vibrating equipment underwent long-term micro-movement: the flanks fretted, the pitch-diameter fit gradually loosened, the preload kept decaying, and the joint had to be retightened frequently.
[Mechanism] Under vibration, fretting on the thread flanks gradually loosens the fit; the accumulated wear grows the clearance and steadily decays the preload into loosening.
[Calculation] Fretting wears the flanks by 0.005mm per month, the pitch diameter grows, the clearance widens, and the preload drops 10% per month.
[Design Omission] The vibrating threads had no anti-fretting measures — a design defect leading to fretting wear and gradual loosening.
1) Treat the threads (phosphate / plating) against fretting;
2) Add anti-loosening features to reduce micro-movement;
3) Refine the thread surface roughness Ra;
4) On first articles, measure wear in a vibration endurance test;
5) Raise the preload to reduce micro-movement;
6) Check tightness on schedule;
7) State the anti-fretting requirement on the drawing;
8) Verify durability.
GB/T 197-2018 General-purpose metric screw threads — Tolerances