E43-790 · Key-and-Spline Fit Error · A drive spline with carburized depth of 0.3mm (should be 0.8mm) gives inadequate tooth-surface hardness support, rapid tooth-side wear under torque, and growing clearance · ★★★
The tooth surface of a drive spline has a carburized layer only 0.3mm deep (design: 0.8mm); the hardened case is thin, the soft core gives inadequate support, tooth-side wear under torque is rapid, and tooth-side clearance grows by 0.02mm per month.
[Mechanism] Spline tooth surfaces rely on the carburized hardened case for wear resistance; a shallow case gives inadequate hard support, rapid tooth-side wear, and growing clearance.
[Calculation] A 0.3mm carburized layer is insufficient: the hardened case wears through easily, tooth-side wear rate doubles, and clearance grows by 0.02mm per month.
[Design Omission] The spline carburized depth is insufficient, a design defect leading to rapid tooth-side wear.
1) Hold spline carburized depth at the design value of 0.8mm;
2) Hold tooth-surface hardness at HRC58~62;
3) On the first part, measure case depth and hardness;
4) Inspect the carburized case metallographically;
5) Keep the flank fit appropriate;
6) Keep the carburizing process stable;
7) Call out case depth and hardness on the drawing;
8) Wear verification.
GB/T 3478.1-2008 Cylindrical involute splines