E43-811 · Key-and-Spline Fit Error · Cold-roll-formed spline profile overshoot causing inaccurate involute, profile interference in mesh with internal spline, binding insertion and rough torque transmission · ★★★
The cold-roll-formed spline had a tooth-profile overshoot (deviated involute); local profile interference occurred in mesh with the internal spline, insertion bound, and under torque the profile contact was uneven and transmission was rough.
[Mechanism] The spline tooth profile must be accurate for proper involute meshing; a roll-forming profile overshoot makes the involute inaccurate, causing interference, binding, and uneven contact.
[Calculation] The profile overshoot locally bulges the involute by 0.03mm, causing interference, binding insertion, and uneven contact.
[Design Omission] Roll-forming profile overshoot; design omission leads to involute interference and binding.
1) Control cold-roll-forming tooth-profile error;
2) Inspect the profile with a spline composite gauge;
3) Trial-insert and check contact on the first article;
4) Maintain roll-tooling accuracy;
5) Check involute contact with bluing;
6) Meet the centering-accuracy requirement;
7) Specify tooth-profile tolerance on the drawing;
8) Insertion verification.
GB/T 3478.1-2008 Cylindrical involute splines