E43-814 · Key-and-Spline Fit Error · Excessive key-side interference in a thin-walled hub causing keyway sidewall burst-stress to exceed the limit when the key is driven in, thin-walled hub cracking along the keyway · ★★★★
The key-side interference in a thin-walled hub was excessive; when the key was driven in, the keyway sidewall burst-stress exceeded the material strength, the thin-walled hub cracked along the keyway root, and the hub was scrapped.
[Mechanism] Key-side interference puts burst-stress on the keyway sidewall; a thin-walled hub is weak, and excessive interference drives the burst-stress over the limit and cracks it.
[Calculation] A 0.05mm key-side interference makes the keyway sidewall burst-stress exceed the thin-walled hub strength, cracking it along the keyway root.
[Design Omission] Excessive key-side interference in a thin-walled hub; design omission leads to bursting.
1) Reduce key-side interference for thin-walled hubs (normal/clearance fit);
2) Check hub stress at the keyway;
3) Thicken the wall at the keyway;
4) Verify no cracking after assembly on the first article;
5) Inspect key width and keyway width;
6) Ensure material toughness meets requirements;
7) Specify key-side fit on the drawing;
8) NDT verification after assembly.
GB/T 1095-2003 Flat keys — Cross-section dimensions for keyways