Knowledge Base › Tolerance and Fit Error Case › Backlash Too Small, Thermal Seizing

Backlash Too Small, Thermal Seizing

E43-835 · Gear-Drive Tolerance Error · A high-temperature gearbox's room-temperature backlash was consumed by gear and housing thermal expansion at high temperature, jamming the teeth and scuffing the tooth faces · ★★★★

Problem Description

A high-temperature gearbox had backlash set at the room-temperature 0.15mm; at high running temperature the differential expansion of gears and housing consumed the backlash, the teeth jammed solid, and with no oil film the tooth faces scuffed.

Root Cause

[Mechanism] At high duty, gear thermal expansion consumes the backlash; if room-temperature backlash is too small, it goes to zero at temperature and the gears seize and scuff.
[Calculation] An 80℃ gear temperature rise expands the tooth thickness and closes the 0.15mm backlash to zero, seizing and scuffing.
[Design Omission] The high-duty backlash left no thermal-expansion margin - a design defect leading to thermal seizing.

Corrective Solution

1) For high duty, size up the backlash for thermal expansion;
2) Thin the tooth thickness to leave hot-state backlash;
3) On first articles, measure backlash hot;
4) Ensure lubrication and cooling;
5) Match material expansion;
6) Design by the duty temperature;
7) Call out hot-state backlash on the drawing;
8) Hot-running verification.

Checklist

Reference

GB/T 10095.1-2022 Cylindrical gears — System of accuracy