E43-838 · Gear-Drive Tolerance Error · A heavy-duty gear's Ra3.2 tooth face was too rough, letting asperities contact and breaking boundary lubrication, scuffing the face under heavy load and high speed · ★★★★
A heavy-duty gear's tooth face at Ra3.2 (should be ≤0.8) was too rough; surface asperities touched directly, the oil film could not form, and under heavy load and high speed the asperities welded and tore, scuffing and scratching the tooth faces.
[Mechanism] The tooth face must be smooth to form an oil film; too rough, asperities pierce the film and contact directly, welding and scuffing under heavy load and high speed.
[Calculation] Ra3.2 leaves asperities taller than the film, boundary lubrication fails, the contact points heat up, and the faces weld and scuff.
[Design Omission] Tooth-face roughness was not controlled - a design defect leading to scuffing.
1) Hold tooth-face Ra ≤0.8 (grind / hone the teeth);
2) Choose anti-scuff gear oil (extreme-pressure additive);
3) On first articles, measure Ra and scuffing;
4) Control tooth-face temperature rise;
5) Harden the tooth face;
6) Modify profile to reduce load;
7) Call out tooth-face Ra on the drawing;
8) Verify under heavy load.