Insufficient Tooth-Face Hardness, Wear and Pitting

E43-842 · Gear-Drive Tolerance Error · A gear's HB220 tooth face (should be HRC58) left insufficient contact fatigue strength and pitted and wore within short running · ★★★

Problem Description

A gear tooth face at HB220 was too soft (designed carburized HRC58); contact fatigue strength was insufficient, and within short running the face pitted, wore, the profile broke down, and transmission noise rose.

Root Cause

[Mechanism] Tooth-face contact fatigue strength relies on hardness; insufficient hardness lowers the allowable contact stress, causing pitting and wear in service.
[Calculation] HB220 has half the allowable contact stress of HRC58; the actual contact stress exceeds allowable, causing pitting and wear.
[Design Omission] Tooth-face hardening was insufficient or a process was skipped - a design defect leading to pitting and wear.

Corrective Solution

1) Carburize and quench the tooth face to HRC58–62;
2) Test hardness;
3) On first articles, check metallurgy and hardness;
4) Check contact stress;
5) Hold case depth to spec;
6) Keep the heat-treatment process stable;
7) Call out tooth-face hardness on the drawing;
8) Verify durability.

Checklist

Reference

GB/T 10095.1-2022 Cylindrical gears — System of accuracy