Gear-Grinding Burn and Tooth-Face Cracks

E43-852 · Gear-Drive Tolerance Error · A ground tooth face burned from excessive grinding parameters, leaving a tempered soft band or grinding cracks that spalled in early service failure · ★★★★

Problem Description

A ground tooth face burned from excessive grinding parameters and inadequate cooling, producing a tempered soft band or grinding cracks; in service the face spalled along the cracks, causing early failure and noise.

Root Cause

[Mechanism] Excessive grinding heat tempers-softens the tooth face or makes grinding cracks, lowering face strength and causing spalling failure in service.
[Calculation] Grinding burn lowers face hardness or leaves tensile-stress surface cracks, cutting contact fatigue strength and causing early spalling.
[Design Omission] Grinding parameters / cooling were wrong and caused burn - a design defect leading to tooth-face spalling.

Corrective Solution

1) Optimize grinding parameters and cool fully to prevent burn;
2) Etch / metallographically inspect for burn and cracks;
3) On first articles, inspect tooth-face quality;
4) Check surface hardness after grinding;
5) Choose the wheel properly;
6) Control grinding heat;
7) Note burn prevention in the process sheet;
8) Verify durability.

Checklist

Reference

GB/T 10095.1-2022 Cylindrical gears — System of accuracy