Wrong Tooth-Thickness Measurement Datum, Misjudgment

E43-855 · Gear-Drive Tolerance Error · A gear's wrong base-tangent span tooth count biased the reading, misjudged tooth thickness, reworked good parts or let out-of-tolerance parts in · ★★★

Problem Description

The wrong number of teeth was spanned for base-tangent measurement, biasing the reading and misjudging tooth thickness as out of tolerance, reworking good parts; or the reverse, letting out-of-tolerance parts be accepted and mixed in.

Root Cause

[Mechanism] Base-tangent tooth-thickness measurement needs the correct span count by tooth number; a wrong count biases the reading and misjudges tooth thickness.
[Calculation] A one-tooth span error biases the base-tangent reading by one base pitch, misreading tooth thickness and misjudging.
[Design Omission] The base-tangent span count was chosen wrongly - a design defect leading to tooth-thickness misjudgment.

Corrective Solution

1) Look up the correct base-tangent span count by tooth number;
2) Cross-check tooth thickness by the ball-pin method;
3) Recheck tooth thickness on first articles;
4) Standardize the measurement procedure;
5) Calibrate the base-tangent micrometer;
6) Call out the base-tangent value and span count on the drawing;
7) Recheck misjudged parts;
8) Verify the fit.

Checklist

Reference

GB/T 10095.1-2022 Cylindrical gears — System of accuracy

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL