Sharpened Tip, Heat-Treatment Cracking

E43-870 · Gear-Drive Tolerance Error · A positive-shift gear's too-sharp tip through-hardened and embrittled during carburizing/quenching, then chipped and spalled in service · ★★★

Problem Description

A profile-shifted gear had tip thickness <0.4m and was too sharp; during carburizing and quenching the sharp tip through-hardened and embrittled, and under service impact the tip chipped and spalled, ruining the profile and making noise.

Root Cause

[Mechanism] An over-sharp tip through-hardens and embrittles during carburizing/quenching, has poor toughness, and chips under impact.
[Calculation] Tip thickness <0.4m lets the sharp corner carburize and through-harden, becomes highly brittle, and chips on impact.
[Design Omission] Too large a shift sharpened the tip - a design defect leading to tip chipping.

Corrective Solution

1) Control the shift coefficient to hold tip thickness ≥0.4m;
2) Chamfer the tip to cut the sharp corner;
3) On first articles, measure tip thickness and hardness;
4) Prevent over-carburizing the tip;
5) Hold material toughness;
6) Check the shift;
7) Call out tip thickness on the drawing;
8) Verify under impact.

Checklist

Reference

GB/T 1356-2001 Cylindrical gears for general and heavy engineering - Standard basic rack tooth profile