E43-880 · Seal-and-Clearance Error · A pump shaft seal journal's roughness designed Ra0.4 but measured Ra1.6 (turned unground) abraded the lip quickly and wept water early · ★★★
A centrifugal-pump shaft seal journal was turned but not finish-ground; roughness Ra1.6 over the Ra0.4 design, and within tens of hours the lip was abraded by the peaks into burr edges, losing seal and weeping water.
[Mechanism] The microscopic peaks/valleys of a rotary shaft act as countless micro-blades; excessive roughness abrasive-wears the rubber lip in relative motion and destroys the seal line.
[Calculation] Lip wear rate ∝ Ra × surface speed; Ra 0.4→1.6 (4×) sharply raises wear, and the seal line widens from a stable μm band and loses seal.
[Design Omission] The journal was turned not ground, with no roughness check - a design defect leading to too-rough surface, lip wear, and leak.
1) Grind the seal journal to Ra0.2~0.4 to remove turning peaks;
2) Make the lay non-directional (plunge grind) to prevent pumping imbalance;
3) Profilometer-measure first-part roughness and file it;
4) Harden the journal HRC≥45 for wear resistance;
5) Choose the process from the Ra-vs-lip-wear relation, quantified;
6) After first-part run-in, check the lip for burrs;
7) Mark Ra and the process (grinding) on the drawing;
8) Re-grind over-rough journals, or plate then grind.
GB/T 13871.1-2022 Rotary shaft lip-type seals — Basic dimensions and tolerances