Knowledge Base › Tolerance and Fit Error Case › Vertical-Boring-Mill Table Thermal Warpage - Flatness Out

Vertical-Boring-Mill Table Thermal Warpage - Flatness Out

E43-333 · Thermal Deformation Uncompensated · A vertical lathe table ∅1600mm in cast iron, designed temperature equalization, measured 12℃ one-sided rise · ★★

Problem Description

Table temperature rise of 12℃ warped it 0.19mm, making flatness go 0.1mm out of tolerance and the workpiece convex.

Root Cause

[Mechanism] One-sided table heating warps it and the rotating face is not flat; the turned surface comes out convex in the middle.
[Calculation] α=10e-6, Δl=10e-6×1600×12=0.192mm≈0.19mm; the warpage drives flatness error to 0.1mm.
[Design Omission] No temperature equalization or compensation — a design defect leading to flatness out of tolerance.

Corrective Solution

1) Add table temperature equalization, holding rise ≤6℃;
2) Add thermal compensation to correct the 0.1mm flatness;
3) Symmetrically place ribs to reduce warpage;
4) Monitor table temperature in real time;
5) Select low-expansion cast iron to cut Δl;
6) Flip the workpiece to cancel middle convexity;
7) Re-check flatness periodically;
8) On first articles, measure flatness and verify ≤0.03mm.

Checklist

Reference

GB/T 11337-2004 Flatness tolerances