Unwelded Reinforcement Pad

E44-979 · Vessel Strength and Wall-Thickness Deficiency · Reinforcement pad · ★★★

Problem Description

Unwelded pad, cracking, leak

Root Cause

[Mechanism] The opening reinforcement pad was not welded to the shell, defeating the reinforcement area; nozzle-zone stress concentration went beyond allowable and cracked.
[Calculation] Nozzle DN150, required reinforcement area A=drδ=154×9=1386mm² (total need incl. F about 5400mm²), the unwelded pad provided 0, and local σ=210MPa exceeded [σ].
[Design Omission] The pad was not welded, no reinforcement check, and no NDE.

Corrective Solution

1) Fully weld the pad to the shell (double-sided continuous weld, 8mm leg), since the unwelded pad gave 0 reinforcement and a sound weld activates it — thus restoring reinforcement;
2) Check the opening reinforcement area (A need ≥5400mm², supplied enough), since under-reinforcement concentrates stress and a correct check provides enough — thus lowering stress;
3) Ultrasonic-check the pad fit (gap ≤0.5mm), since a loose pad is weak and a tight fit bonds it — thus seating it;
4) Switch to an integral reinforcing forging (no pad), since a pad can detach and integral reinforcement is solid — thus reinforcing firmly;
5) Perform MT on the nozzle zone (no cracks), since cracks first show as lines and can be rejected early — thus finding cracks;
6) Run a hydrotest (1.25× design pressure) and confirm no leak by measurement — thus setting strength by data;
7) Control the weld sequence (symmetric skip welding to prevent distortion), since random welding adds stress and sequenced welding is even — thus welding steadily;
8) Write the pad welding and reinforcement check into the process card, since the root cause was the missed weld and unchecked reinforcement — thus locking it in by process.

Checklist

Reference

GB/T 150.1-2011 Pressure vessels

Related model download:Understood the principle and ready to try?Go to MOULDL to download related 3D models and CAD drawings for free »