E44-164 · Seal Leakage · O-Ring Static Seal · ★★
Compression was 35% (should be 15-25%) and took a permanent set, seeping at the joint.
[Over-Compression] Excessive interference causes permanent set.
[Seepage] Lost elasticity breaks the seal and leaks.
[Design Omission] No compression control and a wrong groove — leak.
1) Control the O-ring compression to 15-25% by groove dimensions; 35% took a permanent set and leaked, so control the ratio to keep elasticity;
2) Re-machine the groove depth to standard; a wrong groove caused over-compression, so groove to standard;
3) Choose a temperature- and pressure-rated O-ring material; service beyond material limits deforms it, so select the material;
4) Lubricate on assembly against twisting and cutting; assembly damage leaks, so grease;
5) Periodically check O-ring elasticity and replace; aging deforms it, so replace on schedule;
6) Keep the compression calculation on file; the original was wrongly set, so document it;
7) On trial, verify no seepage; design requirements need actual measurement, so confirm on delivery;
8) Bring compression check into seal design; the over-compression was the root cause of set, so the design must include it.
GB/T 3452.1-2005 Hydraulic-fluid power - Rubber O-ring seals