E44-583 · Seal Leakage · Equipment Sight Glass · ★★
Leakage, sight glass gasket cracked
[Mechanism] Thermal cycling cracks the sight glass gasket.
[Calculation] The crack causes the leak.
[Design Omission] A temperature-resistant gasket was not selected, the bolts were not tightened uniformly and nothing was inspected - the gasket cracked.
1) Change to a temperature-resistant gasket (silicone gasket rated -60 to 200C or PTFE clad); the original gasket embrittled and cracked under thermal cycling with a DeltaT above 80C and leaked, so a temperature-resistant gasket does not crack;
2) Tighten the sight glass bolts evenly (diagonal, torque 20N-m); over-tightening one side crushes the gasket locally and cracks it, so even tightening prevents it;
3) Control the rate of temperature change (heating and cooling at no more than 10C/min); a rapid change generates thermal stress and cracks the gasket, so a slow change prevents it;
4) Select a thicker gasket to accommodate variation (a 2mm soft gasket tolerates the offset); a thin gasket concentrates the stress and cracks, so thickening it helps;
5) Protect the sight glass against impact (a guard shield); mechanical impact cracks the glass, and the shield prevents it;
6) Inspect the gasket for cracks (dye penetrant or visual at every overhaul); cracking progresses gradually and then leaks, so it is inspected;
7) Limit the sight glass diameter (<=150mm reduces the thermal stress); a large diameter has high thermal stress and cracks easily, so limiting the diameter prevents it;
8) Write the temperature-resistant gasket into the assembly card; the original failure to select a temperature class was the root cause of the cracking, so the assembly card closes the loop.
HG/T 21619-2012 Sight Glasses