E44-434 · Two-Phase Flow and Gas Binding · Elbow Gas-Bearing Erosion · ★★
Gas-bearing two-phase flow erodes the outer side of the elbow with pits 1mm deep, wears through in 3 years, and leaks.
[Mechanism] The gas-liquid two-phase flow scours the outer elbow at high speed, cutting pits 1mm deep.
[Calculation] It wears through in 3 years and leaks.
[Design Omission] No wear-resistant elbow and no gas control were provided — the cause of the two-phase erosion.
1) Make the elbow from a wear-resistant alloy or thicken it; gas-bearing two-phase flow erodes the outer side 1mm deep, wears through in 3 years and leaks, so make it wear-resistant;
2) Control the gas fraction to reduce scouring; more gas worsens erosion, so limit it;
3) Line the outer side of the elbow; the outer wall erodes most, so protect it;
4) Check the erosion rate to set the replacement interval; wear-through is a hazard, so schedule replacement;
5) Polish the flow path to reduce turbulence; turbulence increases erosion, so polish it;
6) Periodically measure wall thickness to detect erosion; it progresses gradually, so ultrasonically gauge it;
7) Switch to a large-radius elbow to reduce scouring; sharp elbows erode badly, so use a long radius;
8) Write wear resistance into the design; the original lack of it was the root cause of erosion, so gate it at design stage.
GB/T 5657-2013 Technical specifications for centrifugal pumps