📚 Technical Articles

Knowledge Base › Fluid Systems Error Case › FGD Heat Exchanger Gypsum Fouling

FGD Heat Exchanger Gypsum Fouling

E44-531 · Heat Exchanger Fouling and Insufficient Heat Exchange · Carbon-Steel FGD Heat Exchanger · ★★

Problem Description

Gypsum slurry adhesion, reduced K, blockage, lower efficiency

Root Cause

[Mechanism] Gypsum precipitates from supersaturated solution and adheres to surfaces.
[Calculation] Rf=0.4 lowers K by 40%, blocks 30% of passages, and reduces efficiency.
[Design Omission] Solids content was not controlled and no flushing was provided, so gypsum fouling occurred.

Corrective Solution

1) Control slurry solids content (density 1050-1150kg/m³, solids ≤15%) to prevent supersaturated crystallization; because gypsum precipitates and adheres when supersaturated, and Rf=0.4 lowers K by 40%, blocks 30% of passages and cuts efficiency, controlling solids suppresses crystallization, restores K and preserves heat transfer;
2) Schedule high-pressure flushing (online flush every 24h, intensified flush at Δp>0.1MPa); because fouling reduces flow area and differential pressure rises before full blockage, periodic flushing removes deposits and keeps passages open;
3) Add online K monitoring (alarm on a 10% K drop); because fouling lowers K as the first symptom, well before efficiency collapses, K monitoring gives early warning and guides flushing;
4) Control pH (5.0-5.8, preventing over-alkalinity that promotes CaSO₄ precipitation); because excessive pH intensifies gypsum supersaturation and deposition, pH control suppresses crystallization;
5) Raise flow velocity (≥1.5m/s) to prevent settling; because suspended gypsum particles settle and adhere in low-velocity zones and harden over time, higher velocity reduces residence time and suppresses settling;
6) Use corrosion-resistant materials (rubber lining / 2205 duplex stainless steel); because gypsum slurry contains Cl⁻ that corrodes carbon steel and corrosion pits promote fouling, corrosion resistance extends life and suppresses fouling;
7) Inspect fouling thickness on schedule (bi-monthly thickness measurement / visual); because deposits thicken and worsen K loss and blockage, quantifying thickness guides the flushing interval;
8) Write solids control and flushing into the FGD maintenance procedure; because the original design omitted solids control and flushing, the root cause of gypsum fouling, the procedure closes the loop.

Checklist

Reference

GB/T 151-2014 Heat exchangers