E44-826 · Piping Supports and Thermal Expansion · Pipe Shoe Slide Surface · ★★
Slide surface seized, no sliding, expansion blocked and stress rising
[Mechanism] A seized slide surface blocks the thermal displacement.
[Calculation] Seizing blocks the displacement and raises the thermal stress >40MPa.
[Design Omission] No rust prevention and no lubrication were provided — so rust protection must be added.
1) Remove rust and lubricate the surface (derust + apply heat-resistant grease): because the original seizing blocked the thermal displacement and raised the stress >40MPa, cleaning and lubricating keeps it sliding;
2) Apply a rust-prevention layer (galvanize / stainless-steel the slide surface): because rust seizes it and rust prevention keeps it free, rust protection is applied;
3) Replace with a stainless-steel slide surface (insert a stainless-steel plate): because rust seizes it and replacement frees it, the surface is replaced;
4) Check the sliding clearance (sliding clearance ≥2mm): because a narrow gap seizes and the check keeps it free, the clearance is checked;
5) Monitor the sliding condition (displacement marks, alarm on jamming): because progressive seizing raises the stress and early awareness helps, sliding is monitored;
6) Perform a thermal displacement test (raise the temperature and record the displacement): because the original lack of testing left the seizing undiscovered, the test measures the true displacement, so the test is run;
7) Control moisture to prevent rust (moisture-proofing / drainage): because dampness seizes it and control relieves it, moisture is controlled;
8) Write the derusting and lubrication into the maintenance card: the original lack of rust treatment was the root cause of the seizing, so maintenance controls the work and it slides freely.
GB/T 17116.1-2018 Pipe supports and hangers