E45-439 · Vibration and Mechanical Stress · Level Sensor · ★★
Vibration cracked the interface between the sensor's potting layer and the housing; moisture seeped in and made the circuit fail from damp
[Mechanism] Under thermal expansion and vibration, the potting compound debonds from the housing; cracks let moisture travel along the interface into the cavity.
[Calculation] Vibration drives the interface shear stress beyond the bond strength; a crack 0.05mm wide lets moisture seep in and lowers the insulation.
[Design Deficiency] The potting compound was mismatched with the housing and no adhesion treatment was done.
① Matching compound: choose a potting compound that bonds to the housing → strengthen the interface
② Primer treatment: prime the housing to increase adhesion → prevent debonding
③ Full potting: pot completely with no cavities → eliminate cracks
④ Elastic cushioning: use elastic potting to absorb vibration → reduce shear
⑤ Sealing redundancy: add a seal ring outside the potting → double protection
⑥ Insulation monitoring: alarm on the cavity insulation → early detection
⑦ Cracking verification: confirm with a vibration plus damp-heat test → data confirmation
⑧ Selection standardization: write potting matching into the process spec → control at the source
GB/T 2423.4-2008 Environmental testing for electric and electronic products - Damp heat, cyclic test