E46-010 · Welding Process & Distortion · Pipe Butt Joint · ★★
The fixture was not clamped tight, so the two pipes misaligned by 2mm; the weld shifted to one side of the base metal and lacked fusion
[Mechanism] A loose fixture misaligns the pipe ends; the arc shifts to one side of the base metal and fusion is incomplete.
[Calculation] A misalignment above one quarter of the wall thickness shifts the fusion, and the lack of fusion weakens the joint.
[Design gap] The butt-joint misalignment was not checked.
① Clamp and align with fixtures: clamp the two pipes tight and align them with fixtures to avoid misalignment
② Control the misalignment: keep the butt-joint misalignment within one quarter of the wall thickness to ensure correct positioning
③ Even tacking: space the tack welds evenly to stabilize the joint
④ Check the joint before welding: check the butt-joint misalignment before welding and correct it early
⑤ NDT for lack of fusion: inspect for lack-of-fusion defects by NDT for early detection
⑥ Re-measure after unclamping: re-measure the alignment after releasing the fixture to avoid offset
⑦ Joint verification: confirm the alignment meets the requirement by misalignment measurement
⑧ Standardize process: write the butt-joint requirement into the welding procedure specification (WPS), controlling at the source
GB/T 985.1-2008 Recommended groove for gas welding, shielded metal arc welding, gas-shielded welding and high-energy beam welding