E46-033 · Welding Process & Distortion · Box Girder · ★★
The box girder was not welded in a symmetrical sequence, so it twisted out of tolerance after welding and was hard to assemble
[Mechanism] Asymmetrical welding makes the faces contract unevenly, twisting the girder.
[Calculation] Uneven contraction puts the twist out of tolerance and makes assembly difficult.
[Design gap] A symmetrical welding sequence was not used.
① Symmetrical welding on four faces: weld the box girder symmetrically on all four faces so contraction is uniform
② Segmented skip welding: use segmented skip welding to relieve twisting
③ Fixture restraint: restrain the component with jig tooling to limit displacement
④ Measure twist after welding: measure the twisting distortion after welding and correct early
⑤ Straighten out-of-tolerance areas: straighten the out-of-tolerance areas to restore the correct shape
⑥ Define the welding sequence: establish a clear welding sequence to stabilize quality
⑦ Twist verification: confirm the requirement is met by twist measurement
⑧ Standardize process: write the symmetrical welding sequence into the welding procedure specification (WPS), controlling at the source
GB/T 19866-2005 General principles for welding procedure specification and qualification