E46-179 · Fastening & Anti-Loosening · Volume assembly line · ★★
Bolts for the same drawing came from different batches; the surface-treatment friction coefficients differed greatly, so with the same tightening torque the actual preload scattered and some joints were under-tightened and leaked oil.
[Mechanism] Torque-method preload depends on the friction coefficient; differences in coating or roughness between batches make the K factor fluctuate, so the same torque gives scattered preload.
[Calculation] When K changes from 0.12 to 0.18, the preload at the same torque differs by about 40%, exceeding tolerance and causing under-tightening or over-tightening.
[Design gap] Production started without re-testing the torque coefficient of incoming bolts.
① Incoming re-test: sample-test the torque coefficient K for each batch; return out-of-spec batches or adjust the torque
② Group by batch: group batches with similar K values for the same joint face to reduce scatter
③ Adjust torque: back-calculate the assembly torque from the measured K of each batch
④ Rotation-angle correction: switch critical joints to the turn-of-nut method to reduce dependence on K
⑤ Supplier control: standardize on suppliers with fixed coating and surface-treatment processes
⑥ In-process sampling: periodically measure the actual preload distribution on the assembly line
⑦ Scatter verification: confirm by the preload dispersion that it is within tolerance
⑧ Standardize process: write batch K re-testing into the incoming inspection specification
GB/T 1231-2006 High-strength large hexagon head bolts for steel structures