E46-235 · Bonding and Sealing · Butt-Jointed Plates · ★★
Two plates with a large thickness difference were butt-bonded on a chamfered joint; the adhesive thickness changed abruptly along the section, stress concentrated and cracked at the thick end, and the joint came apart there under load.
[Mechanism] The abrupt change in adhesive thickness makes load transfer uneven; stress concentrates at the end of the thick adhesive layer, which cracks before the rest of the joint.
[Calculation] The thickness difference raises the local stress to several times the average, becoming the starting point of cracks.
[Design gap] No equal-thickness transition or stepped lap was provided.
① Equal-thickness transition: where the thickness difference is large, use a stepped or chamfered transition
② Keep the adhesive even: make the adhesive thickness as uniform as possible
③ Increase the overlap: use a lap to reduce the end stress
④ Choose a tough adhesive: use a high-toughness adhesive to resist stress concentration
⑤ Sample load: run a load-bearing sample test to confirm
⑥ Strength check: perform a tensile test and check for cracking
⑦ Bond verification: confirm by the tensile test that there is no premature cracking
⑧ Standardize process: write the transition design into the drawing
GB/T 7124-2008 Adhesives - Determination of tensile shear strength (rigid material to rigid material)