E46-253 · Machining Process · Drill Bit · ★★
During drilling the cutting fluid only dripped intermittently; the drill edge ran hot and turned blue, and after about 50 holes the main cutting edge had worn by more than 0.3mm, gradually enlarging the bore out of tolerance.
[Mechanism] Insufficient cutting fluid gives the edge poor heat dissipation; the high temperature accelerates abrasive and diffusion wear.
[Calculation] With a supply pressure below 0.3MPa no continuous fluid film forms at the edge zone, and the temperature rises above 200℃.
[Design gap] No minimum fluid supply pressure and flow rate were specified.
① Maintain the supply pressure: set the cutting-fluid pressure above the specified lower limit to form a continuous fluid film
② Ample flow: match the flow rate to the tool diameter, with high flow for large drills
③ Aim the supply: direct the fluid at the cutting zone instead of spraying it broadly
④ Choose the fluid type: select emulsion or extreme-pressure cutting oil according to the material
⑤ Filter clean: filter the cutting fluid to remove chips and prevent secondary scratching
⑥ Edge check: measure the edge wear at intervals and change the tool when it exceeds the threshold
⑦ Wear verification: confirm the wear is under control by a stable bore diameter
⑧ Standardize process: write the fluid supply parameters into the work instruction, controlling at the source
GB/T 6144-2010 Synthetic cutting fluids