E46-276 · Machining Process · Cylindrical Grinder · ★★
A hardened part was left only 0.1mm of grinding allowance (should be 0.3mm); rough grinding already reached size, finish grinding had no stock left, the dimension stuck at the lower limit and the part was prone to burning.
[Mechanism] Insufficient allowance prevents finish grinding from correcting prior errors and easily causes heat burn.
[Calculation] An allowance of 0.1mm is less than the sum of deflection and error, so the size cannot be held.
[Design gap] No adequate post-hardening grinding allowance was specified.
① Leave enough allowance: leave more than 0.3mm of grinding allowance before hardening
② Split rough and finish: rough grinding removes the bulk, finish grinding holds the size
③ Measure the prior stage: measure the blank size before grinding to determine the allowance
④ Control burning: use a small feed and ample cooling for finish grinding
⑤ Check the size: measure the outer diameter after grinding
⑥ Keep a margin: trial-grind the first piece of the batch first
⑦ Dimension verification: confirm the size has been reached with a measuring tool
⑧ Standardize process: write the grinding allowance into the process card, controlling at the source
GB/T 1184-1996 Shape and position tolerances - Undefined tolerances