E46-279 · Machining Process · Machining Line · ★★
The cutting fluid was mixed at only 2% (should be 5%-8%), so the cast-iron parts grew yellow rust after just one day between operations and had to be derusted in a later step.
[Mechanism] Low concentration gives poor rust protection, so the metal surface oxidizes and rusts between operations.
[Calculation] A 2% concentration is below the rust-prevention threshold, and rust appears within hours between operations.
[Design gap] The cutting-fluid concentration was not checked and maintained.
① Control the concentration: keep the cutting-fluid concentration at 5%-8% according to the material
② Test often: test the concentration daily and top up with concentrate
③ Rust-preventive type: use rust-preventive cutting fluid for cast iron
④ Between-operation protection: apply rust-preventive oil between operations
⑤ Change the fluid: change the fluid periodically to prevent spoilage
⑥ Check for rust: check for rust between operations
⑦ Surface verification: confirm by the absence of rust
⑧ Standardize process: write the concentration requirements into the work instruction, controlling at the source
GB/T 6144-2010 Synthetic cutting fluids