Knowledge Base › Process and Assembly Error Case Study › Blunt Reamer Causing Oversized Hole

Blunt Reamer Causing Oversized Hole

E46-282 · Machining Process · Reamer · ★★

Problem Description

A reamer with worn edges was still used; the increased squeezing reamed the hole 0.04mm oversize, so the shaft fit was loose and the clearance was out of tolerance.

Root Cause

[Mechanism] A blunt reamer shifts from cutting to scraping and squeezing, and the sizing section enlarges the hole.
[Calculation] Blunt edges turn reaming from cutting into squeezing, making the hole 0.04mm oversized.
[Design gap] No reamer wear limit or tool-change rule was specified.

Corrective Solution

① Set the limit: set the reamer wear limit for tool change
② Change often: change the reamer as soon as it dulls to keep it cutting
③ Choose the allowance: leave a suitable allowance before reaming
④ Adequate cooling: add cutting fluid when reaming
⑤ Trial ream: ream a test piece first and measure the hole diameter
⑥ Check the hole diameter: measure and confirm after reaming
⑦ Dimension verification: confirm acceptance with a plug gauge
⑧ Standardize process: write the reamer tool change into the process card, controlling at the source

Checklist

Reference

GB/T 1132-2004 Machine reamers with parallel shanks