E46-290 · Machining Process · Machining Line · ★★
A weldment was finish-machined to size without stress relief; it distorted during the subsequent annealing, so the finish-machined dimensions failed and re-machining was needed.
[Mechanism] Welding residual stress is released during annealing; if it is not released before machining, the finish-machined surface distorts.
[Calculation] A part not stress-relieved distorts 0.3mm during annealing, exceeding the finish-machining allowance.
[Design gap] Stress relief before finish machining was not planned.
① Stress-relieve first: anneal after welding to relieve stress
② Sequence control: finish-machine only after stress relief
③ Leave allowance: leave distortion allowance before finish machining
④ Aging: use natural aging when necessary
⑤ Re-measure: re-measure after stress relief
⑥ Clamp securely: clamp securely during machining to prevent distortion
⑦ Dimension verification: confirm stability with measuring tools
⑧ Standardize process: write the stress-relief step into the process route, controlling at the source
GB/T 1184-1996 Shape and position tolerances - Undefined tolerances