E46-388 · Surface Treatment & Coating · Decorative plated part · ★★
The decorative plated part showed rust spots on the surface; high porosity let the substrate rust, so density was poor.
[Mechanism] The coating is thin and porous, so the corrosive medium reaches the substrate and it rusts.
[Calculation] With porosity several times the national standard, salt spray immediately causes rust spots.
[Design gap] The coating thickness and duplex plating were not controlled.
① Control thickness: bring the coating thickness up to spec to reduce porosity
② Duplex plating: use a base coat plus a top coat to increase density and ensure sealing
③ Control pretreatment: clean pretreatment to prevent pores and preserve quality
④ Porosity check: use an iron reagent to check porosity and detect problems early
⑤ Re-plate: thicken and re-plate porous parts to restore density
⑥ Control current: use uniform-current plating to prevent pores and ensure evenness
⑦ Porosity verification: confirm meeting spec with the iron reagent, confirmed by data
⑧ Standardize process: write the plating thickness into the plating process, controlling at the source
GB/T 10125-2021 Corrosion tests in artificial atmospheres - Salt spray tests