Why do stainless fasteners gall (seize), and how do you prevent it?

Austenitic stainless steel (A2/A4) readily forms an oxide film on the surface; without lubrication, at fast tightening speed and excessive temperature, the friction heat in the thread pair causes local fusion welding, producing cold-weld galling. Prevention: (1) apply molybdenum disulfide / wax / a dedicated anti-seize compound at assembly; (2) lower the tightening speed and tighten in stages; (3) do not repeatedly assemble and disassemble the same combination; (4) choose a hardness mismatch (e.g. stainless bolt with a bronze nut); (5) keep the preload torque from being too large. Once galled, do not force it; you can loosen it with local heating (thermal expansion) or coolant + impact vibration; if that fails, destroy and remove it. For stainless grades and properties see the material library mat-01 series; for thread parameters see tb-01. (Note: the fatigue strength of a threaded joint is governed by the stress amplitude; preload that suppresses joint-face opening significantly raises fatigue life. When the clamped parts have low stiffness (soft joint), preload loss is large and a disc spring is needed for compensation. For important joints use ultrasonic force measurement or strain gauges to verify preload rather than relying only on torque, because scatter in the friction coefficient can cause preload fluctuation of +/-25%.)

Related references

tb-01 mat-01

Related 3D models: Ready to build it? Download free 3D models & CAD drawings at MOULDL »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL