How do you select surface treatment for threaded fasteners?

Surface treatment aims at rust prevention, friction reduction and appearance. Common treatments: (1) zinc plating (blue-white / iridescent / black zinc) — general corrosion protection, with hydrogen-embrittlement risk requiring de-embrittlement (mandatory above grade 10.9); (2) Dacromet — high corrosion protection, no hydrogen embrittlement, heat resistant, suitable for automotive and wind power; (3) phosphating + oil — coating base layer, low friction; (4) stainless natural / passivated — food, pharmaceutical, marine; (5) hot-dip galvanizing — thick outdoor protection but affects thread go/no-go gauges. Note that the treatment layer changes the friction coefficient K and thus the torque-preload relationship, so the tightening process must be re-calibrated. For grades and material selection see tb-02; for materials see mat-01. (Note: the fatigue strength of a threaded joint is governed by the stress amplitude; preload that suppresses joint-face opening significantly raises fatigue life. When the clamped parts have low stiffness (soft joint), preload loss is large and a disc spring is needed for compensation. For important joints use ultrasonic force measurement or strain gauges to verify preload rather than relying only on torque, because scatter in the friction coefficient can cause preload fluctuation of +/-25%.)

Related references

tb-02 mat-01

Related 3D models: Ready to build it? Download free 3D models & CAD drawings at MOULDL »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL