Leakage troubleshooting order: (1) confirm the leak location (static or dynamic seal face); (2) static seal — check whether bolt torque is evenly distributed and up to standard, whether the flange face is warped / scored, whether the gasket is offset or aged; (3) dynamic seal — check shaft / piston-rod surface roughness and hardness, runout, scoring, and whether the seal is installed backwards (lip direction) or extruded; (4) medium — is pressure / temperature beyond design, are there abrasive particles; (5) assembly — any ring cutting (use a spiral guide, chamfer to deburr), is the compression enough. Experience: 80% of leakage comes from poor assembly and cleanliness, not the seal itself. For maintenance standards see g-01; for oil-seal parameters see faq-23. (Note: the seal-system design sequence is: first define the service condition (pressure / temperature / speed / medium), then select the type and material, and finally define the groove and compression ratio. Sealing stock must be stored shaded at 0 to 25 C with first-in-first-out; after expiry (NBR about 5 to 7 years) rubber parts lose elasticity, and when compression set exceeds 80% they are unusable.)