Worm-gear drive has large tooth-flank sliding velocity and high friction loss, so efficiency is usually 0.5 to 0.9 (a self-locking worm can be as low as 0.4). Influencing factors: a larger lead angle gamma gives higher efficiency (gamma over 15 degrees is not self-locking, gamma below 5 degrees easily self-locks); more starts give higher efficiency but poorer self-locking; the worm-flank hardness and roughness (hardened and ground Ra 0.4 or below) significantly reduce friction; use a low-friction worm-wheel material (tin bronze ZCuSn10P1) with a steel worm. To improve: choose a multi-start worm, raise worm accuracy and hardness, use extreme-pressure worm-gear oil, and ensure sufficient lubrication and heat dissipation (add fins / cooling). For self-locking duty, sacrifice efficiency for anti-reverse. For material selection see tb-135. (Note: gear strength verification uses two criteria: contact fatigue (pitting) by Hertz stress, bending fatigue by root stress, with safety factors both at 1.2 to 1.5 or above. The face-width factor phi_d is generally 0.8 to 1.4; too large easily causes eccentric loading and needs higher shaft stiffness. A common pairing is a hardened and ground pinion (hard tooth flank) with a soft tooth flank gear, giving good running-in and balanced life.)