How do you choose gear heat treatment (quenching-tempering, carburizing, nitriding)?

Gear heat treatment by load and accuracy: (1) quenching and tempering (quench + high-temperature tempering, hardness 220 to 350 HB) — low-to-medium speed, medium load, soft flank, easy running-in, simple process; (2) surface hardening (induction / flame, flank 45 to 55 HRC) — resists contact fatigue, tough core; (3) carburizing and quenching (flank 58 to 62 HRC, case depth 0.5 to 1.5 mm) — heavy load, impact, high wear, needs grinding; (4) nitriding (surface 500 to 700 HV, little distortion) — high accuracy, light load, no grinding needed, anti-scuffing. Material: quenching-tempering uses 45 / 40Cr, carburizing uses 20CrMnTi, nitriding uses 38CrMoAl. For hardness conversion see tb-146; for process see tb-145. (Note: tooth-flank roughness strongly affects contact fatigue; ground teeth Ra 0.4 to 0.8 are better than hobbed teeth Ra 1.6 to 3.2. High-speed gears need dynamic balancing (G2.5 to G6.3) and a modal analysis of the housing to avoid the meshing frequency. Worm-gear efficiency rises with the lead angle, but a lead angle below 5 degrees is self-locking; design chooses according to need.)

Related references

tb-145 tb-146 tb-135

Related 3D models: Ready to build it? Download free 3D models & CAD drawings at MOULDL »
MOULDL · Mechanical Engineering Knowledge Base · free self-study reference for machine designers, 3D CAD models at MOULDL