The four basic heat treatments: (1) annealing — heat and slow cool, lowers hardness, relieves stress, improves machinability; used as pre-treatment for cast and forged parts; (2) normalizing — air cool, slightly higher strength than annealing, finer structure; often used as pre-treatment or low-demand final treatment; (3) quenching — fast cool to get martensite, very high but brittle hardness; (4) tempering — after quenching, low or medium temperature relieves stress (low 150 to 250 temper keeps hardness, medium 350 to 500 gives spring toughness, high 500 to 650 quenching-tempering gives balanced properties). Quenching-tempering = quench + high-temperature temper. For process temperature and microstructure see tb-145; for hardness correspondence see tb-146. For material see faq-56. (Note: heat-treatment distortion control: reasonable furnace loading, slow heating, choose a medium with uniform martensite transformation (step / isothermal quench); leave machining allowance on complex parts and finish afterward. Hardness inspection per GB/T 230 (HRC), GB/T 231 (HBW); acceptance follows the drawing hardness band, not experience alone.)